聚甲醛日本宝理总代理商-POM总代理商-日本宝理POM聚甲醛产品
POM塑料的型号
1.日本宝理:M90-44,M90-45,M90-04,M90-02,M90-35,M90,M90S,M25S,M25-04,M25-44,M270,M270-44,M270-UP,M90-71,CS-20,GB-25,GC-25,GH-25,GH-25D,GR-20,VC-32,KT-20,SU-25,SW-01,SW-22,SW-41,SX-35,CW-01,SF-20,EB-10,ES-5,FX-11J,NW-02C,NW-02,TR-20,0L-10,U10-01,HP25X
2.美国杜邦:23P,51P,100,100P,4510,500,500AF,500AL,500BK,500CL,500NC,500P,500T,507,507BK,525GR,527UV,570,577,588P,900,900P,90EMP,988P,927UV,DE-20076-NC,DE-20171,DE-20199,DE-20242,DE-20266-BK602,DE-8902,DE-8903,DE-9422,DE-14009-HP,DE-9206BK,DE-20323,DE9422-BK602[2]
⒊德国巴斯夫:2640Z4NC,N2310P,N2720M63,N2640Z6,N2200,N2640Z2,FK61002,H320,S2320
⒋日本旭化成:4520,DG450,GT525,HC750,LA541,LD755,LM511,LT802,SA472,Z4513,AK510,AK751,HC450,LA501,MT754,3010,4013A,4060,4510,4513,4590,5013A,7050,7054,7520,7554,DG400,EF-450,LP402
POM的长期耐热性能不高,但短期可达到160℃,其中均聚POM短期耐热比共聚POM高10℃以上,但长期耐热共聚POM反而比均聚
POM高10℃左右。可在-40℃~100C温度范围内长期使用。
POM极易分解,分解温度为240度。分解时有刺激性和腐蚀性气体发生。故模具钢材宜选用耐腐蚀性的材料制作。
结晶料,熔融范围窄,熔融和凝固快,料温稍低于熔融温度即发生结晶。流动性中等。吸湿小,可不经干燥处理。